Influence of solid phase conductivity and cellular structure on the heat transfer mechanisms of cellular materials: diverse case studies
E Solorzano, MA Rodriguez-Perez, J Lazaro, JA Saja
Advanced Engineering Materials 11, 2009
692009
On the relationship between internal porosity and the tensile ductility of aluminium alloy die-castings
E Lordan, J Lazaro-Nebreda, Y Zhang, K Dou, P Blake, Z Fan
Materials Science and Engineering: A 778, 139107, 2020
382020
Improved degassing efficiency and mechanical properties of A356 aluminium alloy castings by high shear melt conditioning (HSMC) technology
J Lazaro-Nebreda, JB Patel, Z Fan
Journal of Materials Processing Technology 294, 117146, 2021
302021
Alternative carbonates to produce aluminium foams via melt route
J Lázaro, E Solórzano, MA Rodríguez-Pérez
Procedia Materials Science 4, 275-280, 2014
272014
Heat treatment of aluminium foam precursors: effects on foam expansion and final cellular structure
J Lázaro, E Solórzano, MA Rodríguez-Pérez, O Rämer, F García-Moreno, ...
Procedia materials science 4, 287-292, 2014
252014
Improved defect control and mechanical property variation in high-pressure die casting of A380 alloy by high shear melt conditioning
Y Zhang, JB Patel, J Lazaro-Nebreda, Z Fan
JOM 70, 2726-2730, 2018
232018
In-situ microstructural control of A6082 alloy to modify second phase particles by melt conditioned direct chill (MC-DC) casting process–A novel approach
SM KM, NS Barekar, J Lazaro-Nebreda, JB Patel, Z Fan
Journal of Materials Processing Technology 295, 117170, 2021
212021
Effect of solidification rate on pore connectivity of aluminium foams and its consequences on mechanical properties
J Lázaro, E Solórzano, MA Rodríguez-Pérez, AR Kennedy
Materials Science and Engineering: A 672, 236-246, 2016
172016
Effective degassing for reduced variability in high-pressure die casting performance
E Lordan, J Lazaro-Nebreda, Y Zhang, Z Fan
JOM 71, 824-830, 2019
162019
Early anisotropic expansion of aluminium foam precursors
J Lazaro, E Solórzano, JA De Saja, MA Rodríguez-Pérez
Journal of Materials Science 48, 5036-5046, 2013
162013
Solidification processing of scrap Al-alloys containing high levels of Fe
J Lazaro-Nebreda, JB Patel, ITH Chang, IC Stone, Z Fan
IOP Conference Series: Materials Science and Engineering 529 (1), 012059, 2019
152019
Pore connectivity of aluminium foams: effect of production parameters
J Lázaro, E Solórzano, MA Rodríguez Pérez, F García-Moreno
Journal of materials science 50, 3149-3163, 2015
122015
Applicability of solid solution heat treatments to aluminum foams
J Lázaro, E Solórzano, J Escudero, JA De Saja, MÁ Rodríguez-Pérez
Metals 2 (4), 508-528, 2012
122012
High-shear De-Gassing and de-ironing of an Aluminum casting alloy made directly from aluminum end-of-life vehicle scrap
K Al-Helal, J Lazaro-Nebreda, JB Patel, GM Scamans
Recycling 6 (4), 66, 2021
112021
Effect of microstructural anisotropy of PM precursors on the characteristic expansion of aluminum foams
J Lázaro, E Laguna-Gutiérrez, E Solórzano, MA Rodríguez-Pérez
Metallurgical and Materials Transactions B 44, 984-991, 2013
112013
High-pressure die casting: a review of progress from the EPSRC future lime hub
E Lordan, Y Zhang, K Dou, A Jacot, C Tzileroglou, S Wang, Y Wang, ...
Metals 12 (10), 1575, 2022
102022
Advanced casting technologies using high shear melt conditioning
G Scamans, HT Li, JL Nebreda, J Patel, I Stone, Y Wang, X Yang, Z Fan
Fundamentals of Aluminium Metallurgy, 249-277, 2018
102018
Melt conditioned direct chill (MC-DC) casting of AA-6111 aluminium alloy formulated from incinerator bottom Ash (IBA)
KW Al-Helal, J Lazaro-Nebreda, JB Patel, GM Scamans, Z Fan
Recycling 4 (3), 37, 2019
92019
Degassing of aluminum alloy melts by high shear melt conditioning technology: An overview
J Lazaro-Nebreda, JB Patel, E Lordan, Y Zhang, E Karakulak, K Al-Helal, ...
Metals 12 (10), 1772, 2022
72022
Heat transport in closed cell aluminum foams: application notes
J Lazaro, J Escudero, E Solorzano, MA Rodriguez-Perez, JA Saja
Advanced Engineering Materials 11, 2009
72009